Application

Valve actuator

An actuator turns pressure into motion. Its life depends on one bore, one rod and two seals — and the machining of the bore is what decides whether the seals last or weep.

Send a drawing

The cylinder bore

The bore has to be round, straight and on size. A bore that is 0.02 mm oval lets the piston seal leak past, and the actuator drifts under load.

Honing is the usual finish for a cylinder bore: it corrects roundness and sets the crosshatch that retains oil. A bored-only cylinder works, but the seal life is shorter.

FeatureTypicalEffect if missed
Bore diameterH8/H9, 0.02 mmSeal leak
Roundness0.01 mmDrift under load
Straightness0.02 over lengthPiston binds
Surface finishRa 0.2-0.4, crosshatchSeal life
Bore to end face0.05 mm squareUneven cap seal

Rod and piston seals

The rod seal sees the outside world and the piston seal separates the two chambers. Both need a smooth, round counterface and the right clearance.

The rod itself has to be hard and smooth: Ra 0.2-0.4, typically hard chrome plated, with no spiral lead that would pump oil past the seal.

SealCounterfaceNote
Rod sealRod Ra 0.2-0.4, hard chromeNo spiral lead
Piston sealBore Ra 0.2-0.4Honed
End cap O-ringFace flat 0.05Square to the bore
WiperRod, cleanExcludes dirt

End caps and the joint

The end cap seals against the bore and the end face. A face that is not square to the bore lets the cap tilt, and the O-ring loads on one side.

Tie rods or threads hold the assembly together. Threaded caps need a thread concentric to the bore, or the cap tightens off-centre.

Materials and finish

Aluminum for light duty, steel for high pressure, stainless for corrosion. The bore is usually honed regardless of material.

Anodizing a cylinder bore is a mistake on a sealing bore — the coating is hard but it can craze and it changes the dimension. Hard chrome or a honed bare bore is the standard.

MaterialBore finishNote
6061HonedDo not anodize the bore
SteelHonedHigh pressure
316LHoned, passivatedCorrosion
Cast ironHonedDamping

The rod and the gland

The rod is half the seal. It has to be hard, smooth and straight, and it must not have a turning spiral that pumps oil past the rod seal.

That is why rods are usually ground and hard chrome plated rather than turned. A turned rod with a visible lead will leak slowly, and the leak looks like a failed seal.

Rod propertyRequirementNote
Diameterf7 or per sealFit
FinishRa 0.2-0.4Seal life
HardnessChrome platedWear
Straightness0.02 mmBinds the gland
LeadNonePumps oil

FAQ

Why does my actuator drift?
Bore out of round, or a worn piston seal. The bore is the first thing to check.
Does the bore need honing?
For seal life, yes. Honing corrects roundness and sets the crosshatch.
Should the bore be anodized?
No. Hard anodize can craze and changes the dimension on a sealing bore.
What rod finish?
Ra 0.2-0.4, typically hard chrome, with no spiral lead.
Why does the end cap leak?
The end face is not square to the bore, so the O-ring loads unevenly.
Can you hone the bore?
Honing runs through a partner; boring and inspection stay with us.

Have a drawing to review?

Send the model, the revision and the quantity. You get a written review of the open items with the price.

Send a drawing →

Privacy policy