6061-T6 aluminum
6061-T6 is the default aluminum for machined parts, and it earned that position by being unremarkable at everything: it machines well, welds, anodizes evenly and costs less than the high-strength alloys.
Send a drawingWhat the numbers say
Tensile strength 310 MPa, yield 276 MPa, hardness around 95 HB. Density 2.70 g/cm³, about a third of steel. Thermal conductivity 167 W/m·K, which is also why it cuts cool and why heat sinks are made from it.
It is heat-treatable, but T6 is the temper you buy: solution treated and artificially aged. Re-heating it above about 150 °C for long periods starts to overage it and reduce strength.
| Property | 6061-T6 | What it means in the shop |
|---|---|---|
| Tensile | 310 MPa | Fine for brackets and housings, not for high load |
| Machinability | Excellent | Fast cuts, good finish, predictable tool life |
| Anodizing | Very good, even colour | The alloy to choose for cosmetic parts |
| Weldability | Good | Welded frames and enclosures are practical |
| Corrosion | Good, improves when anodized | Not for constant salt immersion |
Where it stops being the right choice
Above about 400 MPa of required strength, 7075-T6 gives 572 MPa from the same envelope. For fatigue-critical parts, 2024-T4 is the traditional choice. For salt water, 5052 or 5083 resist better.
The trap is specifying 6061 for a part that will be hard anodized and loaded: hard anodizing builds 40–50 µm and can embrittle thin sections, so the alloy is not the only decision.
Thin walls and plate stress
6061 plate is rolled and stressed. Machine one face and a long, asymmetric part bows — often more than the flatness callout. The process answer is to rough both faces, release, then finish.
The design answer is to avoid walls under 1.5 mm unless the function needs them. A 1.5 mm wall is usually functionally identical to 0.8 mm and markedly cheaper to produce.
6061 versus the European equivalents
6082-T6 is the European near-equivalent and is common on drawings from Germany and Scandinavia. It machines slightly better and anodizes slightly better than 6061, and its strength is within a few percent.
6083 is a tougher variant used where the part has to absorb impact. If a drawing calls 6082 and only 6061 is in stock, the substitution is usually acceptable for machined parts, but say so on the quote rather than in a phone call.
| Alloy | Tensile | Machinability | Anodizing | Substitution |
|---|---|---|---|---|
| 6061-T6 | 310 MPa | Excellent | Very good | Reference |
| 6082-T6 | 310 MPa | Very good | Very good | Direct for most parts |
| 6083 | 310 MPa | Good | Good | Where toughness matters |
| 6063 | 240 MPa | Excellent | Best of the family | Low-load cosmetic parts |
FAQ
- Is 6061 strong enough for a structural bracket?
- Usually yes if the load path is designed for it. 310 MPa tensile in a 5 mm section carries a lot; the failure mode is usually stiffness and fasteners, not tensile strength.
- Can 6061 be welded after machining?
- Yes, but weld heat distorts a finished part. Weld first, then finish-machine the critical features.
- Why is 6061 cheaper than 7075?
- It is more available, machines faster and is easier to anodize. The price difference is roughly 15–25% in material and less in machining.
- Does 6061 anodize evenly?
- Better than 7075 or 2024. That is why cosmetic enclosures are almost always 6061.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.
Related
6061 vs 7075 — Which alloy, with the numbers.