Material

7075-T6 aluminum

7075-T6 is the high-strength aluminum: 572 MPa tensile, nearly double 6061, at the cost of corrosion resistance and anodizing consistency. It is chosen when load or weight drives the design and 6061 runs out of strength.

Send a drawing

What you gain and what you give up

Zinc and copper are what make 7075 strong, and also what makes it corrode. It is not recommended for sustained salt exposure without a protective finish, and T6 temper is susceptible to stress corrosion cracking under sustained tensile load in a corrosive environment — T73 exists for that reason.

Anodizing is less even than 6061 because of the alloying elements. A cosmetic part in 7075 needs a sample before the batch.

Property7075-T66061-T6
Tensile572 MPa310 MPa
Yield503 MPa276 MPa
MachinabilityGoodExcellent
AnodizingFair, colour can shiftVery good
WeldabilityNot recommendedGood
Relative material cost1.4–1.6×1.0×

Where it belongs

Aerospace brackets,模具 and tooling plates, high-load fixtures, drone frames, bicycle components, climbing hardware — anything where the part must be light and carry load.

It is also common in blow moulds and injection mould tooling because it takes a polish and holds up under cycling pressure.

Machining notes

7075 cuts cleanly but is less forgiving than 6061: it is harder on tools and more prone to chatter in thin sections because it is stiffer and stronger. Rigidity in the fixture matters more.

Stress-relieved plate (often sold as 7075-T651) machines flatter than standard T6, which matters for tooling plates and fixture work.

T6, T651 and T73: which temper

The temper decides residual stress and corrosion behaviour as much as the alloy does. T6 is general purpose; T651 is T6 with a controlled stretch that relieves stress and machines much flatter; T73 is overaged to resist stress corrosion cracking at about 10% less strength.

For a tooling plate, T651 is worth the premium because the plate stays flat after machining. For a structural part in a corrosive environment, T73 is the safe choice. Neither is a machining decision.

TemperYieldResidual stressCorrosionUse
7075-T6503 MPaHighSCC susceptibleGeneral high-strength parts
7075-T651503 MPaLowSCC susceptibleTooling plates, fixtures
7075-T73435 MPaLowSCC resistantAerospace structures

FAQ

Is 7075 worth the extra cost?
Only when 6061 is not strong enough. If a 6061 part is passing, switching to 7075 adds 40–60% to the price for strength you do not need.
Can 7075 be anodized black?
Yes, but the colour is less consistent than 6061 and can go bronze or purple on some batches. Approve a sample.
Is 7075 weldable?
Not practically. Welding 7075 causes cracking in the heat-affected zone. Design for fasteners or adhesive instead.
What is T651?
T6 with a controlled stretch to relieve residual stress. It machines flatter and is the right choice for tooling plates.

Have a drawing to review?