Materials
The alloy decides machinability, finish, corrosion behaviour and price — often more than the geometry does. These are the families we machine, and what changes when you switch between them.
Send a drawingSeven families side by side
| Family | Grades | Machinability | Strength | Corrosion | Relative cost |
|---|---|---|---|---|---|
| Aluminum | 6061, 7075, 5052, 2024, 6082 | Excellent | Low–medium | Good (anodized) | 1.0 |
| Stainless | 303, 304, 316L, 17-4PH | Fair | Medium–high | Excellent | 2.5–4× |
| Steel | 1045, 4140, S45C | Moderate | High | Poor without coating | 1.2–2× |
| Brass | C360, C260 | Excellent | Low | Good indoors | 3–4× |
| Copper | C110, C101 | Poor | Low | Poor (oxidizes) | 4–5× |
| Titanium | Grade 2, Grade 5 | Difficult | Very high | Excellent | 6–10× |
| Plastics | POM, PEEK, PC, ABS, PA, PMMA | Good | Very low | Varies | 0.5–8× |
How to choose, in the order that matters
Start with the constraint that cannot move, then let the rest follow.
| If the binding constraint is… | Choose | Because |
|---|---|---|
| Cost and machinability | 6061-T6 aluminum | Fastest to cut, cheapest to finish, easy to anodize |
| Strength at minimum weight | 7075-T6 or Grade 5 titanium | Strength-to-weight, at 2–4× the machining cost |
| Corrosion in chlorides | 316L stainless | Molybdenum resists pitting where 304 fails |
| Electrical or thermal conductivity | C110 copper | Conductivity is the whole point; machining is secondary |
| Electrical insulation | POM or PEEK | Machined plastic beats a coated metal part |
| Fatigue under cyclic load | 2024-T4 or 17-4PH | Fatigue behaviour, not static strength |
| Wear resistance | Hard anodized aluminum or 17-4PH (H900) | Surface hardness where it rubs |
What we stock, what we order
6061 plate and bar in common thicknesses is stock. 7075, 5052 and 2024 are usually available within a few days. Stainless and titanium are ordered to size; 17-4PH adds a heat-treat step and a week.
If a drawing specifies an unusual thickness or temper, expect material procurement to be the longest part of the lead time. We flag the substitute and its effect on strength or finish before quoting rather than after.
Certificates and traceability
Mill certificates are available for any grade on request, traceable to the heat number. For aerospace and medical supply chains that certificate is part of the documentation package, not an optional extra, and it is worth asking for it at quotation so the paperwork does not delay the shipment.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.
Grade pages
Each grade has its own page with the machining behaviour, the tolerances that are realistic and the traps that make a batch fail.
6061-T6
310 MPa, the machining default. Anodizes evenly.
Read7075-T6
572 MPa. Strength at weight, at a corrosion cost.
Read5052-H32
Marine corrosion, formable, gummy at the cutter.
Read2024-T4
Fatigue strength. Poor corrosion without cladding.
Read304 stainless
18/8 general purpose. Work hardens, not for chlorides.
Read316L stainless
Molybdenum for chlorides, marine and medical.
Read17-4PH
Precipitation hardening to 1,310 MPa. Shrinks when aged.
ReadTi-6Al-4V
Grade 5. Steel strength at half the weight, hard on tools.
ReadC360 brass
Fastest common metal. 3% lead, RoHS limits apply.
ReadC110 copper
101% IACS. Gummy, burrs are a functional defect.
Read1045 steel
Medium carbon, hardens to 55 HRC, cheap and tough.
Read4140 steel
Hardenable through section. Pre-hard 28-32 HRC.
ReadPOM (Delrin)
Machines like brass. Creeps, needs annealing.
ReadPEEK
250 °C service. Anneal before finishing.
Read