PEEK (polyetheretherketone)
PEEK is the engineering plastic you choose when the part has to survive temperature, chemicals or both. It costs 10-20 times POM, machines similarly, and needs annealing to hold a tolerance.
Send a drawingWhat PEEK does
Continuous service around 250 °C, resistance to most solvents and acids, low outgassing and good wear behaviour. It is used in semiconductor equipment, aerospace, medical implants and oil and gas seals.
It is also expensive: 10-20 times POM by volume, and it is abrasive to tooling because of the fibre-filled grades.
| Property | PEEK | POM |
|---|---|---|
| Service temperature | ~250 °C | ~90 °C |
| Tensile | 90-100 MPa | 60-70 MPa |
| Chemical resistance | Excellent | Moderate |
| Relative cost | 10-20x | 1.0 |
| Annealing | Required for tolerance | Recommended |
Annealing is not optional
PEEK machined from extruded stock moves after machining unless it has been annealed. A rough anneal at 200 °C with a slow ramp, then finish machining, is the reliable sequence for tight work.
Finished parts can be stress-relieved after machining, but that risks distortion of thin features. Plan it before the cut.
Machining notes
Sharp carbide, high speed, modest feed, air blast. Glass or carbon-filled grades are abrasive and wear tools quickly; expect shorter tool life and a rougher finish.
PEEK chips are light and static-prone, so extraction matters for cleanliness as well as for the machine.
| Grade | Filler | Effect |
|---|---|---|
| Unfilled | None | Best machinability, lowest strength |
| Glass-filled (GF30) | 30% glass fibre | Stiffer, abrasive, rougher finish |
| Carbon-filled (CF30) | 30% carbon fibre | Stiffer, conductive, very abrasive |
Where it beats metal
A PEEK insulator or wear pad can replace a metal part where electrical insulation, weight or chemical resistance matters more than strength. It also avoids the corrosion problems of stainless in aggressive chemistry.
It does not replace metal where load, stiffness or thermal conductivity are the requirement — PEEK is an insulator, thermally and electrically.
FAQ
- Can you hold 0.05 mm in PEEK?
- Yes on a stable part with annealed stock. Thin sections move and are the real limit.
- Why is PEEK so expensive?
- The polymer itself is expensive and the processing is slow. Material dominates the price.
- Is filled PEEK harder to machine?
- Yes. Glass and carbon fillers are abrasive and shorten tool life noticeably.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.