POM (Delrin / acetal)
POM is the plastic that machines most like a metal: chips curl, the finish comes out clean and the tolerance is respectable. What it does not do is stay where you put it if the blank was not annealed and the part is thin.
Send a drawingMachining behaviour
POM cuts at high speed with sharp tools and air blast cooling. It melts rather than shears if the tool rubs, and a melted edge looks like a torn surface that no parameter change fixes.
Water-based coolant can be absorbed and change dimensions, so air blast is the default. Flood coolant is used only where the part geometry demands it.
| Property | POM | Practical meaning |
|---|---|---|
| Tensile | 60-70 MPa | Stiff for a plastic, weak against metal |
| Machinability | Excellent | Chips curl, good finish |
| Thermal | Melts ~165 °C | Rubs and welds if the tool is dull |
| Moisture | Low absorption | More stable than nylon |
| Tolerance | ~0.05 mm | On a stable, annealed part |
Creep and clamping
POM creeps under sustained load: a chuck tightened at the start of a shift is looser an hour later. That is why plastic parts are held in collets or soft jaws at controlled pressure, and why thin tubes are machined on a mandrel.
The clamp mark is the second problem: a serrated jaw deforms the surface rather than scratching it, and no polishing removes a deformation.
Annealing
Extruded POM carries residual stress. Machining releases it and the part bows or shrinks. Annealing the blank before machining stabilises it; annealing after machining can distort the finished part.
A typical anneal is a slow ramp to about 140-150 °C, hold, then a slow cool. It takes a day, and it is the difference between a part that measures correctly tomorrow and one that does not.
Where POM is the right answer
Insulators, wear pads, gears, bushings, rollers and prototype housings. It runs quietly, needs no lubrication, and is cheap to machine compared with PEEK.
It is the wrong answer where load is high, temperature is above about 90 °C in service, or the part must be painted — POM has poor paint adhesion.
| Material | Tolerance | Use |
|---|---|---|
| POM | 0.05 mm | Wear parts, insulators |
| PEEK | 0.05 mm | High temperature, chemical |
| PC | 0.1 mm | Tough transparent covers |
| Nylon | 0.1 mm | Wear parts, absorbs moisture |
FAQ
- Why did my POM part change size?
- Residual stress released, or moisture absorbed. Anneal the blank and measure 24 hours after machining.
- Can POM be painted?
- Poorly. Adhesion is low. If appearance matters, ABS or PC is a better choice.
- What coolant for POM?
- Air blast. Water-based coolant can be absorbed and change dimensions.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.