Electronics
Electronics enclosures fail on three things: thermal contact, grounding, and the panel that does not fit after anodizing. All three are decided on the drawing, not at assembly.
Send a drawingThe three failure modes
Thermal contact. A heat sink base 0.1 mm out of flat leaves an air gap, and air is an insulator. Base flatness of 0.05 mm over the contact area is the practical specification.
Grounding. Anodizing is an insulator. If a chassis needs a ground path, that area must be masked before coating or machined after it — both change the process and the price.
Panel fit. Anodizing builds 5–25 µm per surface. A connector cut-out that was a comfortable fit becomes tight, and a display window that was flush sits proud.
| Feature | Specification | Effect if missed |
|---|---|---|
| Heat sink base flatness | 0.05 mm | 30–50% worse thermal resistance |
| Grounding pad | Masked or post-machined | No electrical continuity |
| Connector cut-out | Sized after coating | Connector will not seat |
| Panel flatness | 0.1 mm | Visible gap at the bezel |
| Threaded inserts | Masked or re-tapped | Fastener binds or strips |
Materials that make sense
6061 for chassis and panels, 5052 where weight and corrosion matter, copper or C110 for heat spreaders when conductivity is the point, and POM or PEEK for insulators.
Hard anodizing on a chassis gives wear resistance at the cost of 40–50 µm of build — fine for a housing, wrong for a connector face.
What to tell us
Which areas must stay conductive, what the thermal interface is (paste, pad or direct), and the connector datasheet rather than a dimension from a drawing. Connector cut-outs are the most common source of rework because the drawing shows the nominal, not the tolerance stack.
EMI, grounding and the metal that does both
An anodized aluminum chassis is an insulator on every surface. If the design needs EMI shielding or a ground path, the joint between parts has to be conductive: masked anodizing, a conductive gasket, or a machined bare pad.
The cheapest reliable answer is a machined pad, masked before anodizing or cut after coating. Both are specified on the drawing; neither can be added at assembly.
| Requirement | Solution | Effect on price |
|---|---|---|
| Ground path | Masked pad before anodizing | Low, if designed in |
| Ground path, late | Machine the pad after coating | Medium, extra operation |
| EMI seam | Conductive gasket + bare faces | Medium |
| Full shielding | Conductive coating or plated plastic | High |
FAQ
- Why is my heat sink not performing?
- Usually base flatness. A 0.1 mm bow leaves an air gap, and paste cannot bridge it. Specify 0.05 mm over the contact area.
- How do I ground an anodized enclosure?
- Mask the grounding area before anodizing, or machine it after. Masking is cheaper and leaves a cleaner surface.
- Can you anodize after assembly?
- No. Anodizing is a chemical bath; assembled parts trap electrolyte and the finish is uneven. Anodize, then assemble.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.