Surface finishing
Finishing is not cosmetic on a machined part. It changes dimensions, corrosion behaviour and how the part is judged on arrival, and every one of those is decided on the drawing.
Send a drawingWhat each finish does to size
Anodizing converts the surface rather than coating it, and it grows both outward and inward. Powder coating sits on top. Passivation removes contamination and changes nothing dimensionally. That difference decides which fits survive.
The single most common failure is specifying a finish without saying whether the fit is measured before or after it.
| Finish | Build | Effect on a tight bore | Corrosion |
|---|---|---|---|
| Bead blasting | Removes 2-5 um | Slightly larger | None, cosmetic base |
| Anodizing Type II | 5-25 um | Closes 10-50 um on diameter | Good |
| Hard anodizing Type III | 40-50 um | Closes 80-100 um | Very good, wear resistant |
| Powder coating | 60-100 um | Closes holes under 3 mm | Good, thick barrier |
| Zinc plating | 5-15 um | Small, threads usually masked | Sacrificial on steel |
| Nickel plating | 5-25 um | Closes, used on brass | Good, decorative |
| Passivation | None | No change | Restores stainless |
| Laser marking | None | No change | Cosmetic only |
Masking: the manual work nobody quotes
Anodizing is an insulator. A grounding boss, a chassis mating face or a thread used as an electrical path has to be masked before the bath, or machined after it. Both are manual operations and both are priced.
Masking is also where small runs get expensive: a $40 batch charge and ten minutes of hand masking can exceed the value of the parts.
Colour and batch consistency
Anodized colour depends on alloy, bath chemistry, temperature and dwell. Two batches a week apart differ; two different alloys in the same batch differ more. If a panel and a housing must match, they go in the same load, in the same alloy.
Hard anodizing is usually darker and less saturated than Type II, and it cannot be matched to a Type II sample.
| Requirement | Finish | Note |
|---|---|---|
| Cosmetic, colour matched | Type II, same batch | Send a physical sample |
| Wear surface | Type III hard | Dark, matte, builds 40-50 um |
| Outdoor marine | Type II + seal, or powder coat | Sealing matters more than thickness |
| Electrical grounding | Type II with masked pads | Specify the pads on the drawing |
| Food contact | Passivation (stainless) or Type II | Confirm the standard with the buyer |
When finishing changes the process
A part that will be hard anodized cannot have a bore that must stay at H7 after coating — the 40-50 um build closes it. The bore is machined undersize so the finished bore lands in tolerance, which means the shop needs the final dimension, not the pre-plate one.
The same applies to threads, dowel holes and any sliding fit. Say it on the drawing and the process accounts for it; say it after the parts come back and the batch is scrap.
FAQ
- Does anodizing change the thread?
- Yes, the hole tightens by roughly twice the build. Small threads are usually masked or chased with a tap after coating.
- Can you match a colour exactly?
- Within a batch, closely. Across batches there is always a shift; approve a sample from the production batch.
- Is hard anodizing better than Type II?
- It is harder and more wear resistant, but it builds 40-50 um and is more brittle. For a housing it is fine; for a bearing bore it breaks the fit.
- Do you do the finishing in-house?
- Finishing runs through qualified partner shops on the same purchase order, so responsibility for a dimensional change in the tank stays with us.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.
Related
Anodizing vs powder coating — Conversion versus coating.