Process

Hard turning

Hard turning cuts hardened steel with a CBN insert at 45-65 HRC, replacing grinding for many parts. It removes the grinding queue and it holds about 0.01 mm — but it leaves a different surface than grinding does.

Send a drawing

What it replaces

A hardened shaft or a bearing seat that used to be ground can be turned with CBN in one pass, in the same setup as the rest of the part. That saves the grind, the re-chuck and the queue.

It does not replace grinding where the roundness or the surface integrity requirement is extreme, or where the part is a precision bearing race.

RequirementHard turningGrinding
Size 0.01 mmYesYes
Roundness 0.005 mmDifficultYes
Ra 0.4YesYes
Ra 0.1NoYes
White layer controlNeeds careControlled
Setup changesOne setupSeparate machine

White layer and residual stress

Hard turning generates heat at the edge and can leave a thin white layer — re-hardened, brittle martensite — plus tensile residual stress. On a fatigue-critical part that is a crack initiation site.

The control is the tool condition and the parameters: a worn CBN insert overheats the surface. For safety-critical parts, the surface is specified and sometimes verified by etching or X-ray diffraction.

Parameters and setup

Speeds are high for the material — 150-250 m/min is normal — with a small depth of cut and a low feed. The machine has to be rigid and the part has to be supported, because the cutting force on a hardened surface is significant.

CBN is expensive and brittle. Interrupted cuts and vibration destroy it, so a keyway or a cross-hole in the hardened zone is a reason to grind instead.

MaterialHardnessSpeedNote
4140 / 104545-55 HRC150-220 m/minStandard hard turning
Bearing steel58-62 HRC120-180 m/minCareful white layer control
Case hardened58+ HRC surface120-180 m/minDepth of case matters
Tool steel60-65 HRC100-150 m/minCBN or grinding

FAQ

Can hard turning replace grinding?
For many parts, yes — 0.01 mm and Ra 0.4 are achievable in one setup. For extreme roundness or surface integrity, grinding remains.
What is a white layer?
A re-hardened, brittle surface layer from excessive heat in hard turning. It is a fatigue risk on critical parts.
Can you hard turn an interrupted cut?
It is difficult. A keyway or cross-hole causes impact that destroys CBN.

Have a drawing to review?

Send the model, the revision and the quantity. You get a written review of the open items with the price.

Send a drawing →

Privacy policy