Part family

Dies and punches

A die and punch pair is a cutting tool: the punch pushes the material into the die and the clearance between them decides whether the edge is sheared cleanly or torn. It is a tooling part, so its tolerance and its wear life both matter.

Send a drawing

Clearance is the whole design

The gap between punch and die, expressed as a percentage of material thickness, is what makes a clean cut. Too little clearance and the material tears and the tool wears; too much and the edge rolls and burrs.

Typical clearance for mild steel is 5-8% of thickness per side; for aluminum 4-6%; for stainless 8-10%. Get it wrong and the part has a burr that no deburring operation will fix economically.

MaterialClearance (per side)Edge
Aluminum4-6% of thicknessClean, some burr
Mild steel5-8%Clean
Stainless8-10%Harder to shear
Brass4-6%Very clean
High strength steel10-12%Wear risk

The cutting edge and how it wears

The punch and die edges are sharp, and they wear on the flank. A worn edge needs more force, produces a bigger burr and eventually chips — and a chipped edge marks every part after it.

Dies are reground when the edge wears, which changes the height and sometimes the clearance. That is why a die is designed with grinding stock and why the regrind is part of the tool’s life plan.

Wear stageSymptomAction
NewClean edge, small burrRun
Light wearSlightly larger burrMonitor
ModerateBurr grows, force risesRegrind
HeavyEdge roundingRegrind or replace
ChippedMark on every partReplace insert

Materials and hardening

D2 and A2 are the common cold-work die steels; M2 and powder metallurgy steels for higher wear; carbide for very high volume. All are hardened and tempered, usually to 58-62 HRC.

The hardening has to be done after machining with the distortion allowance left, and the die opening is usually finished by wire EDM after hardening so the edge is not disturbed by a cutter.

MaterialHardnessWearUse
A258-60 HRCGoodGeneral dies
D258-62 HRCVery goodHigh volume
M260-64 HRCExcellentAbrasive material
Powder metal steel60-64 HRCBestVery high volume
Carbide88-92 HRAHighestSpecial

Wire EDM for the die opening

A hardened die opening is cut by wire EDM, which leaves no cutter marks and no heat-affected edge beyond a few microns. The taper can be cut in the same pass, so the die gets its relief angle without a second operation.

The alternative is to mill the opening soft, harden, then grind. That works for simple shapes and is cheaper on a large die where wire EDM time would be prohibitive.

MethodWhenNote
Wire EDM after HTComplex or preciseNo cutter marks
Mill soft, harden, grindSimple, largeCheaper
Sinker EDMBlind or 3DElectrode needed
Jig grindingRound featuresVery accurate

Punch and die alignment

The punch has to enter the die with the clearance held on every side. That means the punch and die are aligned by guide pins and a guide plate, not by the press.

A misaligned punch cuts on one side and rubs on the other, which wears both and produces an uneven burr. The alignment is a tooling job, and it is checked by feeler gauge or by the part’s burr pattern.

ElementFunctionRequirement
Guide pinsAlign punch to die0.01 mm
Guide plateHold the punch squareParallel
StripperHold the materialEven pressure
Backing plateSupport the punchFlat
ShimSet the punch heightMatched

Tolerances and inspection

The die opening and the punch are held to 0.005-0.01 mm and the clearance is set by the pair. After assembly the clearance is checked on a sample part: the burr height and the edge quality tell you whether it is right.

That is the practical inspection — a die is proved by the parts it makes. The dimensional checks come first, but the acceptance is a good edge on a test strip.

FeatureTypicalChecked by
Die opening0.005-0.01 mmCMM, pin gauge
Punch size0.005-0.01 mmMicrometer
ClearancePer materialTest strip
Parallelism0.005 mmSurface plate
Edge qualityPer part specVisual, burr height

What to send, and what we make

Send the part drawing, the material and thickness, the press or the die set if it exists, and the expected volume. Those four decide the clearance, the steel and whether the die is a simple block or a guided set.

Machining of die blocks, punches, strippers and backing plates is done here; hardening and wire EDM run through partners, with the dimensions and the clearance checked before and after.

Maintenance and the cost of neglect

A die that is run past its edge life costs more than the regrind. The force rises, the press works harder, the burr grows and eventually a chipped edge marks a batch of parts before anyone notices.

A regrind schedule based on part count is normal. For a die that runs continuously, the burr height is checked every shift and the die comes out when it exceeds the limit.

MaintenanceIntervalEffect
Burr checkPer shiftDetects wear early
RegrindPer count or burrRestores edge
Clearance checkAfter regrindEnsures quality
Guide lubricationPer shiftWear and seizure

Strippers, pilots and the parts that make a die work

The cutting elements are only part of the tool. A stripper holds the material flat while the punch withdraws, so the part does not lift and bend. A pilot enters a pre-pierced hole to locate the strip before the next station.

Those parts wear too, and they are made to the same standard as the punch. A worn stripper lets the material lift and the part bends; a bent pilot mislocates every part after it.

For a progressive die, the strip layout and the station sequence are part of the design, and the die blocks are machined to that layout. A die that is geometrically correct but has the wrong station spacing will not run.

ElementFunctionWear
PunchCuts the profileFlank and edge
Die blockCuts the clearance sideFlank and edge
StripperHolds the stripFace and springs
PilotLocates the stripDiameter
Guide pinAligns the setDiameter and bore

Repair, spare inserts and the economics of a die

A die is a capital tool, and its cost is spread over the parts it makes. The repair strategy matters as much as the design: a die built with replaceable inserts can be repaired in a day, one built as a solid block may need a new block.

The usual compromise is replaceable cutting inserts on the most-worn stations and a solid block elsewhere. That keeps the common failure cheap to fix without rebuilding the whole tool.

Spare punches are worth holding. A chipped punch stops production, and the lead time for a replacement is days. Holding one spare of each critical punch costs a fraction of a stopped press.

StrategyRepair timeCost
Solid blockDays or new blockHigh
Replaceable insertsHoursMedium
Spare punches heldMinutesLow, small stock
Full spare die setMinutesHighest, rare

FAQ

What is die clearance?
The gap between punch and die, as a percentage of thickness — 5-8% for mild steel, 8-10% for stainless.
Why does my die produce a big burr?
Clearance wrong, edge worn, or punch and die misaligned.
Can a die be repaired?
Yes, by regrinding. A chipped edge may need a new insert.
What steel for a die?
A2 or D2 for general work, M2 or powder metal steel for high volume.
Why wire EDM the die opening?
After hardening it cuts without disturbing the edge and can cut the taper in one pass.
Do you make complete die sets?
Die blocks, punches, strippers and backing plates. Hardening and wire EDM through partners.
How is the die proved?
By the parts it makes — burr height and edge quality on a test strip.
How often is a die reground?
On part count or when the burr exceeds the limit, whichever comes first.

Have a drawing to review?

Send the model, the revision and the quantity. You get a written review of the open items with the price.

Send a drawing →

Privacy policy