Stainless steel turning
Stainless is where turning earns its money and where it punishes bad parameters. The material work-hardens under the tool, so a pass that rubs instead of cuts leaves a surface harder than the one underneath it.
Send a drawingWork hardening in one paragraph
Stainless hardens when it is deformed. A cutter that rubs the surface deforms it without removing it, and the top few microns can reach twice the bulk hardness. The next pass then cuts a hard skin over soft metal, which destroys tool life and finish.
The counter-intuitive rule: keep the feed per revolution high enough that the edge stays under the hardened layer, and never let the tool dwell. A stainless part turned at a light feed with a dull insert is a part that will be scrapped.
Grade choice decides everything
303 contains sulfur, which breaks chips and makes it the free-machining stainless. It is the right default for turned fittings, shafts and spacers — and the wrong choice for food, medical or chloride service, because the sulfur lowers corrosion resistance.
304 and 316L are the corrosion grades and machine 40-50% slower. 316L adds molybdenum for chlorides. 17-4PH machines like a medium steel but shrinks 0.04-0.06% when aged, so the sequence has to be planned before the first cut.
| Grade | Speed (carbide) | Feed | Character |
|---|---|---|---|
| 303 | 150-200 m/min | 0.10-0.20 mm/rev | Free machining, lower corrosion resistance |
| 304 / 304L | 90-140 m/min | 0.08-0.15 mm/rev | General purpose, galls on threads |
| 316 / 316L | 80-120 m/min | 0.08-0.15 mm/rev | Chloride resistance, slower still |
| 17-4PH (annealed) | 80-120 m/min | 0.08-0.12 mm/rev | Heat treat after roughing, shrinks |
Insert geometry, not just grade
A honed edge that works well on steel will rub on stainless. The right geometry is a sharp, positive-rake edge with a coating that resists built-up edge, and a chip breaker sized for the feed you are running.
Coolant has to reach the edge. Through-tool or high-pressure coolant is not a luxury here: it is the difference between a tool that lasts a shift and one that lasts an hour.
Threads and galling
A stainless thread will gall — cold-weld and tear — when assembled dry against another stainless part. That is a material property, not a machining defect, and it is why stainless fasteners are often supplied with a lubricant or a different alloy.
Cut threads rather than rolled on small parts; rolled threads work-harden and can crack. And specify a lubricant on the drawing if the joint will be assembled and disassembled in service.
| Thread | Method | Note |
|---|---|---|
| M6 x 1 internal | Tap, sharp spiral flute | Chase after any coating |
| M10 x 1.5 | Tap or thread mill | Thread mill is more reliable at depth |
| NPT / BSP | Tap + gauge | Sealing thread, gauge required |
| Small 0-80 / M2 | Cut tap only | Rolled threads crack in stainless |
FAQ
- Why does my 304 part work harden?
- Because the tool rubbed instead of cutting. Increase feed per revolution, sharpen or change the insert, and make sure coolant reaches the edge.
- Is 303 acceptable for a food application?
- Usually not. The sulfur improves machinability and reduces corrosion resistance. 304 or 316L is the correct choice even though it costs more to machine.
- Can you turn 17-4PH to a tolerance?
- Yes, but plan the sequence: rough, age, then finish. Ageing shrinks the part by roughly 0.04-0.06%, which will consume a 0.05 mm tolerance if the finishing happens first.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.