Laser marking
Laser marking puts a permanent mark on a part without touching it. On metal the mark is either an annealed oxide colour change or an engraved groove — and the two are not interchangeable.
Send a drawingAnnealing versus engraving
Annealing uses a defocused beam to heat the surface, which changes its colour without removing material. It leaves a surface that is still smooth, which matters on a sealing face or a sliding surface.
Engraving vaporises material and leaves a groove 10-50 µm deep. It is more visible and more permanent under wear, and it is a stress riser on a fatigue part.
| Method | Depth | Surface | Use |
|---|---|---|---|
| Annealing | None | Smooth, coloured | Stainless, titanium, anodized |
| Engraving | 10-50 µm | Grooved | Serial numbers, deep marks |
| Bleaching | None | Light on dark | Black anodized parts |
| Colour change | None | Depends on alloy | Decorative |
Marking anodized aluminum
On black anodized aluminum, a laser can bleach the dye to produce a white mark, or cut through to the substrate for a darker one. Both are permanent and both are done after anodizing.
Marking before anodizing buries the mark under the oxide and it fades. The sequence is machine, anodize, mark.
Data matrix and traceability
A UDI or a data matrix code has to be readable after the part has been through finishing, and it has to survive the part’s service life. Cell size, contrast and the marking method all matter.
The usual requirements are a grade of B or better on the ISO/IEC 15415 scale, verified with a reader rather than by eye. Ask the customer for the grading requirement before marking thousands.
| Mark | Typical size | Requirement |
|---|---|---|
| Data matrix (UDI) | 3-6 mm | Grade B or better |
| Serial number | Character height 1.5-3 mm | Legible after finish |
| Logo | Per design | Contrast after anodize |
| Part number | Per drawing | No confusion with revision |
FAQ
- Does laser marking remove material?
- Annealing does not. Engraving removes 10-50 µm.
- When do you mark an anodized part?
- After anodizing. Marking before buries the mark under the oxide.
- Can a data matrix survive finishing?
- Yes, if it is marked after finishing and verified with a reader.
Have a drawing to review?
Send the model, the revision and the quantity. You get a written review of the open items with the price.